Scrap & Stone Grapple Tines: Hardfacing vs. Replacement?

The biggest problem with Scrap (Orange Peel) and Stone Grapples is that the tine tips melt and shorten due to friction. As the tine gets shorter, gripping ability decreases.
1. Hardfacing or Replacement?
When the tine wears out, you have two options:
- Hardfacing Welding: A temporary solution. The surface is filled with hardfacing electrodes. However, if the base metal is weak, the weld won't hold.
- Tip Replacement: The healthiest method. The worn tip is cut off and a new tip of Hardox 450/500 quality is welded in its place.
2. Importance of Using Hardox
Tines made of ordinary steel melt in 1 week during scrap loading. As HKM, we only use certified Swedish steel (Hardox) for grapple repairs and tip replacements.
Related products
More in this category
Recent articles
Global Mining Report: Cost Analysis in Hard Rock 26 November 2025
Electric Heavy Machinery is Coming: Are Attachments Compatible? 26 November 2025
5 Ways to Save Fuel in Heavy Machinery While Prices Rise 26 November 2025
Noise Pollution Laws and Silent Demolition Technologies 26 November 2025
Future of Construction: "Green Sites" and On-Site Recycling Trend 26 November 2025
Why Made in Turkey? The "Golden Ratio" Between China & Europe 26 November 2025
Our Warranty Policy: Assurance Against Manufacturing Defects 26 November 2025
How Are Your Products Shipped? Safe Packaging for Sea & Air 26 November 2025